ΧΒГ chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of ΧΒГ

Location » Home » Grades > Special Alloy > ΧΒГ

ГОСТ ΧΒГ

Profile

This page is mainly introduced the ΧΒГ chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of ΧΒГ,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
  • Steel Garde:ΧΒГ
  • Type:Special Alloy
  • Country:Russia
  • Standard:ГОСТ
  • Application:Carbide for cutting tools

Chemical composition(mass fraction)(wt.%)

Mechanical Properties

Tensile strength 169~420 σb/MPa
Yield Strength 461 σ 0.2 ≥/MPa
Elongation 02 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 358~299 -
HRC 30 -

Physical Properties

Thermal expansion 86-13 e-6/K
Thermal conductivity 50-30 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 0899-7867 째C
Density 5992-8190 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
ΧΒГ Special Alloy Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk

Technical specification/standard for download