140Cr2 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of 140Cr2

Location » Home » Grades > Special Alloy > 140Cr2

DIN 140Cr2

Profile

This page is mainly introduced the 140Cr2 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of 140Cr2,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
140Cr2
  • Steel Garde:140Cr2
  • Type:Special Alloy
  • Country:Germany
  • Standard:DIN
  • Application:Cold working alloy tool steel

Chemical composition(mass fraction)(wt.%)

Mechanical Properties

Tensile strength 422~864 σb/MPa
Yield Strength 285 σ 0.2 ≥/MPa
Elongation 21 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 205~273 -
HRC 30 -

Physical Properties

Thermal expansion 85-13 e-6/K
Thermal conductivity 43-36 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 5500-8997 째C
Density 6599-1633 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
140Cr2 Special Alloy Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk