T75Cr280 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of T75Cr280

Location » Home » Grades > Special Alloy > T75Cr280

STAS/SR T75Cr280

Profile

This page is mainly introduced the T75Cr280 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of T75Cr280,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
T75Cr280
  • Steel Garde:T75Cr280
  • Type:Special Alloy
  • Country:Romania
  • Standard:STAS/SR
  • Application:Cast Steel

Chemical composition(mass fraction)(wt.%)

Mechanical Properties

Tensile strength 758~418 σb/MPa
Yield Strength 500 σ 0.2 ≥/MPa
Elongation 75 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 866~606 -
HRC 30 -

Physical Properties

Thermal expansion 91-18 e-6/K
Thermal conductivity 03-41 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 0112-2455 째C
Density 2903-6049 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
T75Cr280 Special Alloy Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk

Technical specification/standard for download

Hot keywords:T75Cr280
Previous: T70MoCr280