C67W chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of C67W

Location » Home » Grades > Tool Die Steels > C67W

DIN C67W

Profile

This page is mainly introduced the C67W chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of C67W,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
High carbon steel

Chemical composition(mass fraction)(wt.%)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.64  0.72
Si 0.15  0.40
Mn 0.60  0.80
P   0.035
S   0.035

Mechanical Properties

Tensile strength 045~431 σb/MPa
Yield Strength 832 σ 0.2 ≥/MPa
Elongation 03 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 411~541 -
HRC 30 -

Physical Properties

Thermal expansion 44-42 e-6/K
Thermal conductivity 59-73 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 0205-3768 째C
Density 4721-5293 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

√

√

√

√

√

Size Availability

Steel Grade Specification Processing range(mm)
C67W Tool Die Steels Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk