This page is mainly introduced the SUS 317 L chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of SUS 317 L,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
Stainless steel bars

Chemical composition(mass fraction)(wt.%)

Elements Min.(≥) Max.(≤) Similar Remarks
C   0.08
Si   1.00
Mn   2.00
P   0.045
S   0.03
Cr 18.00  20.00
Ni 11.00  15.00
Mo 3.00  4.00
N  

Mechanical Properties

Tensile strength 245~169 σb/MPa
Yield Strength 588 σ 0.2 ≥/MPa
Elongation 48 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 159~623 -
HRC 30 -

Physical Properties

Thermal expansion 50-55 e-6/K
Thermal conductivity 96-14 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 8669-6553 째C
Density 1499-5095 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
SUS 317 L Stainless Steels Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk