Х25Н16Г7АР chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of Х25Н16Г7АР

GOST Х25Н16Г7АР

Profile

This page is mainly introduced the Х25Н16Г7АР chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of Х25Н16Г7АР,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
Russia GOCT Standard vacuum smelting casting high temperature alloy bar

Chemical composition(mass fraction)(wt.%)

Elements Min.(≥) Max.(≤) Similar Remarks
C   0.12
Si   1.00
Mn 5.00  7.00
P   0.035
S   0.020
Cr 23.00  26.00
Mo  
Ni 15.00  18.00
N 0.30  0.45
B   0.010

Mechanical Properties

Tensile strength 590~680 σb/MPa
Yield Strength 877 σ 0.2 ≥/MPa
Elongation 50 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 176~780 -
HRC 30 -

Physical Properties

Thermal expansion 53-95 e-6/K
Thermal conductivity 87-56 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 5078-6807 째C
Density 2205-8876 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
Х25Н16Г7АР Stainless Steels Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk