T20825 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of T20825

Location » Home » Grades > Tool Die Steels > T20825

UNS T20825

Profile

This page is mainly introduced the T20825 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of T20825,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
Hot-Work Tool Steel

Cross Reference Table(Equivalent Materials):

Material Standard Country
T20825 UNS USA

Chemical composition(mass fraction)(wt.%)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.22  0.32
Si 0.15  0.40
Mn 0.15  0.40
P   0.030
S   0.030
Cr 3.75  4.50
Mo  
V 0.40  0.60
W 14.00  16.00
Ni+Cu   0.75

Mechanical Properties

Tensile strength 433~348 σb/MPa
Yield Strength 694 σ 0.2 ≥/MPa
Elongation 36 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 163~156 -
HRC 30 -

Physical Properties

Thermal expansion 68-55 e-6/K
Thermal conductivity 78-49 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 3887-2033 째C
Density 7202-9350 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
T20825 Tool Die Steels Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk

Technical specification/standard for download

Hot keywords:T20825
Previous: H24
Next: H25