CARPENTER 20 Cb 3 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of CARPENTER 20 Cb 3

UNS CARPENTER 20 Cb 3

Profile

This page is mainly introduced the CARPENTER 20 Cb 3 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of CARPENTER 20 Cb 3,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
Wrought Nickel and Nickel-Related Alloys

Chemical composition(mass fraction)(wt.%)

Elements Min.(≥) Max.(≤) Similar Remarks
C   0.07
Si   1.00
Mn   2.00
P  
S  
Ni 32.00  38.00
Cr 19.00  21.00
Al  
Cu 3.00  4.00
Ti  
Fe   remaining
Mo 2.00  3.00
Co  

Mechanical Properties

Tensile strength 276~080 σb/MPa
Yield Strength 298 σ 0.2 ≥/MPa
Elongation 37 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 566~797 -
HRC 30 -

Physical Properties

Thermal expansion 46-71 e-6/K
Thermal conductivity 61-14 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 2928-0587 째C
Density 8872-9509 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
CARPENTER 20 Cb 3 Stainless Steels Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk