ASTM A335 GRADE P11 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of ASTM A335 GRADE P11

ASTM ASTM A335 GRADE P11

Profile

This page is mainly introduced the ASTM A335 GRADE P11 chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of ASTM A335 GRADE P11,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.
ASTM  A335

Seamless Ferritic Alloy Steel Pipe for High-Temperature Service
  • Steel Garde:ASTM A335 GRADE P11
  • Type:Special Alloy
  • Country:USA
  • Standard:ASTM
  • Application:Seamless Ferritic Alloy Steel Pipe for High-Temperature Service

Chemical composition(mass fraction)(wt.%)

Mechanical Properties

Tensile strength 798~924 σb/MPa
Yield Strength 218 σ 0.2 ≥/MPa
Elongation 31 δ5≥(%)
ψ - ψ≥(%)
Akv - Akv≥/J
HBS 168~322 -
HRC 30 -

Physical Properties

Thermal expansion 27-47 e-6/K
Thermal conductivity 82-92 W/m.K
Specific heat 450-460 J/kg.K
Melting temperature 4142-6572 째C
Density 0038-6888 kg/m3
Resistivity 0.50-0.60 Ohm.mm2/m
     

Heat Treatment Regime

Annealing

Quenching

Tempering

Normalizing

Q & T

Size Availability

Steel Grade Specification Processing range(mm)
ASTM A335 GRADE P11 Special Alloy Round Bar and Hollow Bar Φ1 to Φ2000
Square and Flat Steel Φ10 to Φ100
Plate and Sheet 0.08-800(Thickness)*10-1500(Width)*Length
Tube or Pipe OD:Φ4-410; WT:1-35 mm; Lenght:10-12000
Coil and Strip Steel THK:0.1mm Width:1500mm
Forged Ring/Cylindrical/Disk